Surface Appearance
There shall be no foreign particles embedded into the plastic surface as a result of the extrusion process.
There shall not be any surface distortions that penetrate either internally or externally into the conduit wall greater than 10% of the minimum wall thickness.
There shall not be any holes, visible cracks or defects that could cause damage or compromise the physical strength of the conduit.